The Effect Of Pressure On The Quality Of Magnesia Brick

Date:2016-06-01 11:42 From:Zhengzhou Sunrise Refractory Author:admin
Due to the low plasticity and low moisture content of clay materials, the molding pressure has a big effect on the quality of magnesia brick
Magnesia Brick
If the pressure is too low, the green boady will be not dense, porous and weak and not easy to sintere. The properties of products will be reduced too. 
 
The drying of the green body is not only the water evaporation process and but also the hydration process of magnesia particles. So, the drying stress should ensure the formation of minimum amount of hydrates when removing the moisture. In order to avoid the formation of cracks during the drying process, reasonable drying system should be made. 
 
After drying, the moisture content should be no more than 0.3%. then fire the green body in down draft kilns. The firing temperature is 1550-1600 degree. 
 

Inquiry:

If you have any questions or good suggestions on our products and site, or if you want to know more information about our products, please write them and send to us, a representative will contact you within one business day. We guarantee that your information will not be divulged to the third party.

Title:
Name:
Tel:
*E-mail:
Country or Region:
*Message:
    
If you're interested in the product, please submit your requirements and contacts and then we will contact you in one day. We promise that all your informations won't be leaked to anyone.